The best selling brand of this character known to the author, was made as follows:

225 pounds extra selected American zinc oxide;

225 "

Missouri floated barytes;

50 "

refined linseed oil;

500 pounds paste.

Note. In order to manipulate this with such a small percentage of oil, it was necessary to give the material a good chasing under a powerful wheel.